Aanalytical Modeling of Cutting Tool Wear for Superalloy and Experimental Validation

Lixin Wang, Binglin Li
Vol. 7, No. 3, pp. 90-99, 2025 DOI: 10.54691/bwp7xc95 March 19, 2025
Download PDF
Abstract.Tool life in superalloy cutting is an important parameter that affects the machining cost and efficiency. In this paper, the wear analysis model of superalloy GH901 cutting tool is established by using minimum energy method. The influence of chip velocity, cutting temperature and positive pressure on the wear are considered. Aiming at three different types of cutting tools, the cutting speed of 40m/min is used to carry out the turning wear experiment on superalloy GH901. The tool life curve is established according to the measurement data of the wear width of the back tool face. The analysis and comparison with the literature model prediction and the experimental results show that the proposed model has a good prediction effect on the wear measurement of superalloy tool. Furthermore, the influence of cutting speed and thermodynamic parameters between tool and workpiece on tool wear are analyzed theoretically.
Keywords. Carbide Tool; Flank Wear; Superalloy; Life Prediction.
APA Citation Lixin Wang, Binglin Li (2025). Aanalytical Modeling of Cutting Tool Wear for Superalloy and Experimental Validation. Scientific Journal of Technology, 7(3), 90-99. https://doi.org/10.54691/bwp7xc95

References

  1. Zhang Yanan, Niu Shen, Ming Pingmei, et al. Experimental Research on Micro-Pit Array by Jet Electrochemical Machining on GH4169 Nickel-Based Superalloy[J]. Aeronautical Manufacturing Technology, 2024, 67(18): 54-59.
  2. Usui E, Shirakashi T, Kitagawa T. Analytical prediction of cutting tool wear[J]. Wear, 1984, 100(1-3): 129-151.
  3. JIANG Zenghui, SONG Yazhou, JIA Minfei, et al. Research on Simulation of Carbide Tool Wear in Cutting High-Strength Steel Based on The Usui Model[J]. Manufacturing Technology and Machine Tool, 2019, (5): 112-115.
  4. Zhang X, Yu T, Xu P, et al. In-process stochastic tool wear identification and its application to the improved cutting force modeling of micro milling[J]. Mechanical Systems and Signal Processing, 2022, 164: 108233.
  5. Yan Fugang, Lv Yafei, Li Yanguo, Liu Li,Cheng Yaonan, et al. Analysis of High Temperature Wear Process Mechanism of Cemented Carbide Tool[J]. Tool Engineering, 2017, 51(04): 22-27.
  6. Deng Yadi, Li Binglin, Zhang Rui, et al. Experimental Testing and Theoretical Modeling of Tool Wear in Turning GH901 Superalloy[J]. Mechanical Science and Technology for Aerospace Engineering, 2023, 42(12): 2079-2084.
  7. Thakur D G, Ramamoorthy B, Vijayaraghavan L. Study on the machinability characteristics of superalloy Inconel 718 during high speed turning[J]. Materials and Design, 2009, 30(5): 1718-1725.
  8. Bhatt A, Attia H, Vargas R, et al. Wear mechanisms of WC coated and uncoated tools in finish turning of Inconel 718[J]. Tribology International, 2010, 43(5-6): 1113-1121.
  9. He Yan, Ling Junjie, Wang Yulin, et al. In-Process Tool Wear Monitoring Model Based on LSTM-CNN[J]. Chinese Journal of Mechanical Engineering, 2020, 31(16): 1959-1967.
  10. Akhtar W, Sun J, Sun P, et al. Tool wearmechanisms in the machining of Nickel based super-alloys: A review[J]. Frontiers of Mechanical Engineering, 2014, 9: 106-119.
  11. Huang Y, Liang S Y. Modeling of CBN tool flank wear progression in finish hard turning[J]. J. Manuf. Sci. Eng., 2004, 126(1): 98-106.
  12. Pálmai Z. Proposal for a new theoretical model of the cutting tool's flank wear[J]. Wear, 2013, 303(1-2): 437-445.
  13. Chang Hao, Ma Lianjie, Wan Xuewen, et al. Study on Wear Model for Cutting Tools of Machinable Ceramic[J]. Mechanical Science and Technology for Aerospace Engineering, 2020, 39(1): 83-87.